The extended drawing of wire rod leads to wire cracking
21 Feb,2025
Non-metallic inclusion inspection is performed under a 100x optical microscope for inclusion rating.
View more
What is the maximum allowable shortage of coal mining machine picks?
08 Jan,2025
The number of missing coal mining machine picks must not exceed 10% of the total. This is because coal mining machine picks are important tools in the coal mining process, and an excessive number of missing picks will affect coal mining efficiency, coal seam quality, and the service life of the coal mining machine.
View more
Quality Standard for Diamond Composite Sheet Body Drill Bits
08 Jan,2025
The sintered body drill bit maintains its diameter, using polycrystalline artificial diamond that meets the strength requirements for oilfield use specified by US company Zheng. The alloy used is YG11, suitable for rocks with an F coefficient > 11. After sintering, the surface of the drill bit body must be free from defects such as mesh-like cracks, looseness, etc., that could affect the embedding of cutting teeth.
View more
Precautions for using troughing rollers
08 Jan,2025
Conveyor belts of different types and specifications should not be joined together; the joint should preferably be glued.
View more
A Brief Discussion on the Heat Treatment Technology of Build-Up Welding Rods
24 May,2019
The process performance of crack-free welding rods. The welding rod uses Ni80Cr20 type electric furnace wire as the core wire, and is coated with a metal-graphite type coating. Although no ore powder (marble, rutile, mica, etc.) that plays a role in arc stabilization, slag formation, and gas generation is added to the coating, a large amount of flake graphite (C) is added to the coating. The graphite not only plays a lubricating and plasticizing role during the pressing of the welding rod, but also during the welding process, most of the C is oxidized to generate CO (or CO2) gas to displace the air in the arc column area and protect the molten metal.